ASTM D4072 Standard Test Method for Toluene-Insoluble (TI) Content of Tar and Pitch
1. Scope
1.1 This test method covers the determination of toluene-insoluble matter (TI) in tar and pitch.
1.2 Since this test method is empirical, strict adherence to all details of the procedure is necessary.
1.3 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.
1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use. For specific hazard information, see Section 7.
1.5 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.
2. Referenced Documents
2.1 ASTM Standards:
D95 Test Method for Water in Petroleum Products and Bituminous Materials by Distillation
D362 Specification for Industrial Grade Toluene (Withdrawn 1989)
D850 Test Method for Distillation of Industrial Aromatic Hydrocarbons and Related Materials
D4296 Practice for Sampling Pitch
E11 Specification for Woven Wire Test Sieve Cloth and Test Sieves